Transfer and service stress checks for PT slabs (Class U, T and C)
Stress checks are the serviceability core of a post-tensioned design. What to check at transfer and in service, the ACI 318-19 classes and limits, the Eurocode 2 equivalents, and how the result drives the bonded reinforcement.
Unlike reinforced concrete, a post-tensioned member is checked for concrete stresses at two stages: at transfer, when the prestress is applied to young concrete with little load on it, and in service, when the long-term losses have occurred and the full design loads act. The checks confirm that the concrete is not crushed or cracked more than intended, and they decide how much bonded reinforcement the slab needs. Strength is checked separately (see ultimate strength and secondary moments).
The stress equation
For a section under effective prestress P, eccentricity e and applied moment M, the fibre stresses (compression positive) are:
f = P/A ± P e / S ∓ M / S → in load-balancing form: f = P/A ± Mnet / S
In the load-balancing method, the balancing load cancels part of the applied load, and only the net (unbalanced) moment Mnet produces bending stresses. The hyperstatic (secondary) moments from prestress are included in Mnet because they are real moments in the structure. Design programs report these stresses along design strips or sections.
ACI 318-19 classes
ACI 318-19 §24.5.2 classifies prestressed flexural members by the extreme fibre tension ft in the precompressed tensile zone at service loads, with gross section properties:
- Class U (uncracked): ft ≤ 0.62√f'c (MPa).
- Class T (transition): 0.62√f'c < ft ≤ 1.0√f'c.
- Class C (cracked): ft > 1.0√f'c.
Two-way slabs are designed as Class U with ft ≤ 0.5√f'c (§8.3.4.1 / §24.5.2.1). Class U and T sections use gross properties for deflection; Class C requires a cracked-section analysis and crack control (§24.3.2, §24.2.3.8).
ACI 318-19 permissible stresses
At transfer (§24.5.3), before time-dependent losses:
- Compression: 0.60f'ci generally, 0.70f'ci at the ends of simply supported members.
- Tension: 0.25√f'ci generally, 0.50√f'ci at the ends of simply supported members; where exceeded, bonded reinforcement is provided to resist the total tensile force in the concrete (§24.5.3.2.1).
In service (§24.5.4), for Class U and T members, after all losses:
- Compression under prestress plus sustained load: 0.45f'c.
- Compression under prestress plus total load: 0.60f'c.
Bonded reinforcement in two-way slabs
Even when the stresses pass, ACI 318-19 §8.6.2.3 requires minimum bonded reinforcement in two-way PT slabs:
Positive moment areas, if ft > 0.17√f'c: As,min = Nc / (0.5 fy)
Negative moment areas at columns: As,min = 0.00075 Acf
Nc is the resultant tensile force in the concrete under service loads, and Acf is the larger gross cross-sectional area of the slab-beam strips in the two orthogonal equivalent frames intersecting at the column. The column-area bars are placed within 1.5h either side of the column faces, with at least four bars in each direction (§8.7.5.3).
Indicative values. The ACI 318-19 coefficients in this section are well established, but clause numbering changed between the 2014 and 2019 editions. Check each against the edition adopted for your project.
Eurocode 2 limits
EN 1992-1-1 treats prestress stresses differently:
- At transfer (§5.10.2.2): concrete compression limited to 0.6fck(t); if it exceeds 0.45fck(t), non-linear creep should be considered.
- In service (§7.2): compression limited to k1fck (0.6fck recommended) in exposure classes XD, XF and XS where needed to avoid longitudinal cracks, and to k2fck (0.45fck) under quasi-permanent loads to keep creep linear.
- Cracking (§7.3, Table 7.1N): for unbonded tendons, crack width limits as for reinforced concrete (0.3 mm recommended for most exposure classes under quasi-permanent loads); for bonded tendons, 0.2 mm under frequent loads with a decompression check in XD/XS exposure.
- Tendon stress (§7.2(5)): mean stress in the tendons limited to 0.75fpk after losses.
Many UK designers using TR43 also apply flexural tension limits for unbonded PT slabs (TR43 lists allowable stresses broadly in line with BS 8110 Class 2 and 3 practice). In the UAE and Saudi Arabia, projects often follow ACI 318 for the stress checks and the Dubai or Sharjah regulations for precompression and deflection. Sharjah, for example, requires a vibration check where the span exceeds 42 times the slab thickness (see floor vibration).
Worked example (illustrative)
Slab 220 mm, f'c = 40 MPa, P/A = 1.15 MPa (from our precompression example), net service moment at midspan Mnet = 18 kNm/m (sagging).
S = b h² / 6 = 1000 × 220² / 6 = 8.07 × 106 mm³/m
Mnet/S = 18 × 106 / 8.07 × 106 = 2.23 MPa
Bottom fibre: 1.15 − 2.23 = −1.08 MPa (tension) Top fibre: 1.15 + 2.23 = 3.38 MPa (compression)
Class U limit for two-way slabs: 0.5√40 = 3.16 MPa. The tension of 1.08 MPa is well within it. But 0.17√40 = 1.075 MPa, and 1.08 MPa just exceeds it, so ACI 318-19 §8.6.2.3 requires positive-moment bonded reinforcement. Nc is the area of the tension block times the average tension:
Depth of tension zone y = h × ft / (ft + fc) = 220 × 1.08 / (1.08 + 3.38) ≈ 53 mm
Nc = 0.5 × 1.08 × 53 × 1000 ≈ 28.6 kN/m → As = 28 600 / (0.5 × 420) ≈ 136 mm²/m
Compression of 3.38 MPa is far below 0.45f'c = 18 MPa. At transfer, with only self-weight acting and the initial force perhaps 10 to 15 percent higher, the top fibre at midspan may go into slight tension under the upward balancing load; that is checked against 0.25√f'ci.
Common mistakes
- Checking transfer with the effective (long-term) force rather than the initial force.
- Using f'c instead of f'ci at transfer, or stressing before the transfer strength is confirmed.
- Ignoring restraint from walls and columns, which reduces the precompression actually delivered (see temperature and restraint cracking).
- Averaging stresses over too wide a design strip, hiding peaks at columns.
- Mixing cube and cylinder strengths when converting between codes.
Summary
| Check | ACI 318-19 | EN 1992-1-1 |
|---|---|---|
| Transfer compression | 0.60f'ci (0.70 at simply supported ends) | 0.6fck(t) |
| Transfer tension | 0.25√f'ci (0.50 at simply supported ends) | Crack control by reinforcement |
| Service tension, two-way slab | 0.5√f'c (Class U) | Crack width / decompression, Table 7.1N |
| Class U / T / C boundaries | 0.62√f'c / 1.0√f'c | — |
| Service compression | 0.45f'c sustained, 0.60f'c total | 0.45fck quasi-permanent, 0.6fck characteristic |
| Minimum bonded steel | Nc/(0.5fy) if ft > 0.17√f'c; 0.00075Acf at columns | §7.3.2 minimum areas |
All units MPa with cylinder strengths. Our PT design review checks every strip at transfer and service.
Part of our PT design guides. Codes are referred to by clause where we are confident of the reference, and coefficients marked indicative should be checked against the code text; always check the edition and national annex adopted for your project. Worked examples are illustrative, not designs.
Questions we are asked about this.
What are Class U, T and C in ACI 318?
Classes for prestressed flexural members based on the service tensile stress: U (uncracked) up to 0.62√f'c, T (transition) up to 1.0√f'c, and C (cracked) above that. Two-way slabs are designed as Class U with a lower limit of 0.5√f'c.
What is the tension limit for a PT slab at transfer?
ACI 318-19 limits tension at transfer to 0.25√f'ci, or 0.50√f'ci at the ends of simply supported members. Where it is exceeded, bonded reinforcement must carry the tensile force.
When does a PT slab need bonded bottom reinforcement?
Under ACI 318-19, in positive moment areas where the service tension exceeds 0.17√f'c, with As = Nc/(0.5fy). Bonded top reinforcement of 0.00075Acf is required at columns regardless.
Which prestress force is used for transfer checks?
The initial force after immediate losses (friction, wobble, anchor seating, elastic shortening), before long-term losses.
How does Eurocode 2 check PT slab stresses?
It limits compression at transfer to 0.6fck(t), in service to 0.45fck under quasi-permanent loads (and 0.6fck in some exposures), and controls cracking through crack width or decompression limits in Table 7.1N.
Do stress checks replace strength checks?
No. Stresses are a serviceability check; flexural strength with secondary moments, shear and punching are checked separately at the ultimate limit state.
Technical information only. This article is general engineering information to help you understand the subject. It is not design advice for a specific project, codes and authority requirements change, and worked examples are illustrative. Designs must be prepared and checked by a qualified structural engineer responsible for the project, to the code edition adopted for the project. Disclaimer · Terms of use.
Send the drawings. Get an answer from our engineers.
WhatsApp or email the architectural or structural set, the location and what you need. The reply comes from the engineers who will do the work, with a proposed scope and programme.
- +971 52 118 2569
- Telephone
- +971 52 118 2569
- Office
- Al Warqa 1, Dubai, UAE
- Hours
- Sunday – Thursday, 09:00 – 18:00 GST