1. Home
  2. Resources
  3. Fire resistance of PT slabs
PT design guide  ·  Iron Axis engineering team

Fire resistance of post-tensioned slabs (EN 1992-1-2 and BS 8110)

Prestressing strand loses strength at lower temperatures than reinforcing bars, and an unbonded tendon heated at one point loses force along its whole length. How fire resistance is designed into PT slabs, what the tabulated methods require, and what to check after a fire.

Design codes
ACI 318 · Eurocode 2 · PTI
Software
RAM Concept · AutoCAD · Revit

Concrete protects steel in a fire because it heats up slowly. The deeper the steel sits, the longer it takes to reach a temperature at which it loses strength. Prestressing strand is cold-drawn high-strength steel, and it loses strength at lower temperatures than hot-rolled reinforcement; it also relaxes rapidly when hot. For that reason fire codes require PT slabs to have more cover (axis distance) to the tendons than an equivalent reinforced concrete slab, and designers need to think about how the slab behaves when one part is heated.

Who sets the fire rating

The required fire resistance period comes from the fire code, not the structural code. In the UAE that is the UAE Fire and Life Safety Code of Practice issued by the Civil Defence, which sets ratings by building type, height and occupancy; in Saudi Arabia, the Saudi Building Code SBC 801 (Fire). The structural engineer then shows that the slab achieves that rating, usually by tabulated data (EN 1992-1-2 §5, BS 8110-2 Section 4, or ACI 216.1), and occasionally by simplified or advanced calculation.

Why PT slabs are more sensitive

  • Critical temperature. EN 1992-1-2 §5.2 uses a critical temperature of about 350 °C for prestressing wires and strands and 400 °C for prestressing bars, against 500 °C for reinforcing bars, which is why the axis distance is increased.
  • Unbonded tendons. An unbonded tendon heated locally relaxes and loses force along its whole length, which can reduce load balancing in spans that were not heated. Bonded tendons lose strength only where they are hot.
  • Thin slabs. PT slabs are slender, so heat reaches a larger part of the section. Minimum thicknesses in the tables address this and the separating function (insulation, I).
  • Restraint. Thermal expansion of the heated slab pushes on surrounding structure. Restraint can help (by arching action and increased compression) or harm (by pushing columns and walls); see temperature and restraint.

EN 1992-1-2 tabulated data for flat slabs

For flat slabs (slabs supported on columns without beams), EN 1992-1-2 §5.7.4 and Table 5.8 give a minimum slab thickness hs and minimum axis distance a to the bottom reinforcement. For prestressing steel, §5.2(5) requires the axis distance to be increased by 10 mm for prestressing bars and 15 mm for prestressing wires and strands.

EN 1992-1-2 Table 5.8 flat slabs, with the strand increase (indicative)
Fire ratingMinimum slab thickness hsAxis distance a, reinforcing barsAxis distance, strands (a + 15 mm)
REI 60180 mm15 mm30 mm
REI 90200 mm25 mm40 mm
REI 120200 mm35 mm50 mm
REI 180200 mm45 mm60 mm
REI 240200 mm50 mm65 mm

Table 5.8 also requires, for REI 90 and above, that at least 20 percent of the total top reinforcement in each direction over intermediate supports is continuous over the whole span and placed in the column strip. The axis distance is measured from the exposed surface to the centre of the strand (not to the sheathing). Ductile concrete detailing and the National Annex may adjust the values.

Indicative values. The Table 5.8 values and the 15 mm strand increase are quoted from EN 1992-1-2 as we understand it. Check the current edition and the National Annex for your project before using them.

BS 8110-2 and TR43

BS 8110-2 Section 4 gives tabulated minimum dimensions and covers for fire resistance, with separate, larger values for prestressed members; for flat slabs the covers increase with the rating, and the tables distinguish simply supported and continuous members. BS 8110 has been superseded in the UK by Eurocode 2 but is still used on some regional projects. TR43 refers designers to the Eurocode tables for post-tensioned floors. ACI 216.1 provides the US equivalent, with cover tables for restrained and unrestrained prestressed slabs.

Worked check (illustrative)

A flat slab needs REI 120. EN 1992-1-2 Table 5.8 gives hs ≥ 200 mm and a = 35 mm; with strands, a = 35 + 15 = 50 mm to the strand centre. For a 12.7 mm monostrand with sheathing about 15 mm in diameter:

Clear cover to the sheathing at the low point ≈ 50 − 7.5 = 42.5 mm
Compared with a 25 mm durability cover, the low point rises by about 17.5 mm

In a 220 mm slab that loses roughly 12 percent of the drape, so the force needed to balance the same load rises by about the same proportion (see precompression and balanced load and tendon profile and layout). This is why the fire rating needs to be fixed before the tendon layout.

Spalling

Explosive spalling exposes tendons directly to the fire. It is more likely with high-strength concrete, high moisture content, dense mixes and high compressive stress. EN 1992-1-2 §4.5 says spalling is unlikely for concrete with moisture content below 3 percent by weight in the tabulated method, and §6.2 adds requirements for high-strength concrete (for example polypropylene fibres). Precompression raises the compressive stress, which is one more reason to keep it within sensible limits.

After a fire

  • Do not core, drill or cut tendons until the slab has been assessed. A heated tendon may have lost force and strength, and its anchorage may be compromised (see openings and coring).
  • Assess the extent of heating from damage indicators: colour change of the concrete, spalling depth, deformation, and the condition of finishes and services.
  • For unbonded tendons, check the tendon force (lift-off tests) in heated areas and in adjacent spans along the same tendons.
  • Take cores or samples away from tendons for laboratory testing where needed.
  • Design repairs or strengthening, which may include replacing tendons; our structural strengthening design service covers this.

Summary

Fire resistance of PT slabs
ItemRuleReference
Required ratingSet by the fire code for the buildingUAE Fire and Life Safety Code; SBC 801
Critical temperature, strandsAbout 350 °C (bars 500 °C) (indicative)EN 1992-1-2 §5.2
Axis distance increase+15 mm strands and wires, +10 mm prestressing bars (indicative)EN 1992-1-2 §5.2(5)
Flat slab minimumsREI 60 180/15 to REI 240 200/50 mm (indicative)EN 1992-1-2 Table 5.8
Continuity at supportsREI 90+: 20% of top steel continuous in column stripEN 1992-1-2 Table 5.8
SpallingMoisture < 3% for tabulated method; HSC rulesEN 1992-1-2 §4.5, §6.2
AlternativesBS 8110-2 Section 4; ACI 216.1Regional practice

We check fire covers and their effect on the tendon profile in every PT design review.

Part of our PT design guides. Codes are referred to by clause where we are confident of the reference, and coefficients marked indicative should be checked against the code text; always check the edition and national annex adopted for your project. Worked examples are illustrative, not designs.

S-430 FAQ

Questions we are asked about this.

Do PT slabs need more fire cover than RC slabs?

Yes. Prestressing strand loses strength at lower temperatures, so EN 1992-1-2 §5.2(5) increases the axis distance by 15 mm for strands and wires and 10 mm for prestressing bars.

What slab thickness is needed for a 2-hour fire rating?

For flat slabs, EN 1992-1-2 Table 5.8 gives a minimum of 200 mm for REI 120, with an axis distance of 35 mm for bars, or about 50 mm for strands. Check the edition and National Annex.

Are unbonded tendons worse in a fire?

An unbonded tendon heated locally loses force along its whole length, which can affect spans that were not heated. Bonded tendons lose strength only where they are hot.

Who decides the fire rating of a slab?

The fire code sets it: the UAE Fire and Life Safety Code in the UAE and SBC 801 in Saudi Arabia. The structural engineer shows that the slab achieves it.

Can a PT slab be reused after a fire?

Often, after assessment. Tendon force, concrete condition and anchorages are checked, and repairs or strengthening designed where needed.

Does fire cover affect the PT design?

Yes. Larger axis distance reduces the drape, so more prestress force is needed to balance the same load. The fire rating should be fixed before the tendon layout.

S-901 Contact

Send the drawings. Get an answer from our engineers.

WhatsApp or email the architectural or structural set, the location and what you need. The reply comes from the engineers who will do the work, with a proposed scope and programme.

Office
Al Warqa 1, Dubai, UAE
Hours
Sunday – Thursday, 09:00 – 18:00 GST